TY - EJOU AU - Gu, Jierong AU - Hua, Licheng AU - Xie, Shuangquan AU - Shen, Xiang AU - Xu, Tiefeng AU - Liu, Zijun TI - High Hardness Ge45As40Se15 Glasses Based on Ball-Milling and Chalcogenide Glasses Molded by Spark Plasma Sintering T2 - Chalcogenide Letters PY - VL - IS - SN - 1584-8663 AB - In this work, Ge45As40Se15 chalcogenide glass was prepared using spark plasma sintering. This method synthesizes glass powder into blocks through a certain temperature and pressure, which is an effective densification and high-precision molding of infrared transparent blocks and lenses. Through X-ray diffraction (XRD) and differential scanning calorimetry analysis, we tracked the gradual evolution of the powder during ball milling and observed the existence of a glass transition temperature in the glass after powder hot pressing. This method can prepare components outside the conventional glass forming region with high hardness and infrared transmittance, providing a simple and economical synthetic approach for preparing chalcogenide glass materials with optical application potential. KW - Chalcogenide glass; spark plasma sintering; glass forming region; high hardness DO - 10.32604/cl.2026.086724